Difficulty Analysis and Solutions for Flux Residues

"Flux residue during reflow soldering of low-temperature solder paste" refers to a certain amount of flux remaining on solder joints or in the soldering area because the flux used in the soldering process cannot be completely volatilized or decomposed during reflow soldering with low-temperature solder paste.
Jul 6th,2026 129 Views

Flux Residues: Difficulty Analysis and Solutions

What is flux residue?
Why does flux residue occur?
How to deal with flux residue?
In an electronic manufacturing factory, they started using a new type of low-temperature solder paste for reflow soldering. When they began using this new low-temperature solder paste, they noticed flux residue problems on some solder joints. These residues formed obvious white spots around the solder joints, affecting the reliability and appearance of the solder joints. Let's take a closer look~

What is Flux Residue

"Flux residue during reflow soldering of low-temperature solder paste" refers to a certain amount of flux remaining on solder joints or in the soldering area because the flux used in the soldering process cannot be completely volatilized or decomposed during reflow soldering with low-temperature solder paste.
When flux residue occurs during reflow soldering of low-temperature solder paste, it may bring the following impacts:
  • Electrical Performance Issues: Flux residue may negatively affect the electrical performance of solder joints and circuit boards. Flux residues can cause short circuits or poor conductivity between circuit boards, thereby affecting the normal function of the circuit. In addition, flux residue may also affect the stability and reliability of solder joints, leading to increased resistance or failure of solder joints.
  • Reliability Issues: The presence of flux residues may negatively affect the reliability of soldered connections. Flux residue can cause corrosion, metal ion migration, or oxidation of solder joints, thereby reducing their reliability. This may lead to solder joint breakage, loosening, or failure under high temperature or vibration conditions.
  • Cleaning Difficulties: If flux residue is difficult to remove, it may increase the complexity and difficulty of the cleaning process. If the residues cannot be completely removed, it may adversely affect subsequent process steps, such as coating, encapsulation, or testing. In addition, the presence of residues may also reduce the surface adhesion after cleaning, affecting the quality of subsequent coating or bonding.
  • Appearance and Visibility Issues: Flux residue may leave unclean traces or bubbles on the soldered surface. This may affect the appearance quality of the product and reduce the visibility of solder joints. In some applications where appearance and visibility are important factors, flux residue may be regarded as a quality issue.

Causes of Flux Residue

The following are some factors that may cause flux residue:
  1. Inappropriate Flux Composition: Low-temperature solder paste usually uses a lower-temperature soldering process, while traditional high-temperature fluxes may contain flux components that are difficult to completely volatilize or decompose during low-temperature soldering. Therefore, it is crucial to select a flux compatible with low-temperature solder paste to ensure that the flux can be properly volatilized or decomposed during reflow soldering.
  2. Improper Temperature Control: Low-temperature solder paste needs to be reflowed within an appropriate temperature range to ensure solder joint quality and complete volatilization of flux. If the reflow temperature is too high or too low, the flux may not be completely volatilized or decomposed, leading to the formation of residues.
  3. Material Mismatch or Quality Issues: Quality problems with low-temperature solder paste, flux, or other related materials may also cause flux residue. For example, if the selected low-temperature solder paste is incompatible with the flux used, or the material itself has quality problems, it may cause the flux to fail to completely volatilize or decompose.

Solutions

Some measures to control flux residue:
  • Control Reflow Soldering Parameters: Correctly control the temperature and time parameters of reflow soldering to ensure that the flux can be fully volatilized and decomposed. Excessively high temperature may lead to incomplete volatilization of flux, while excessively low temperature may fail to melt and decompose the flux. Adjust the temperature profile and time of the reflow oven according to the requirements of low-temperature solder paste and flux.
  • Optimize the Cleaning Process: Thoroughly clean the soldered PCB to remove flux residue. Select appropriate cleaning agents and cleaning methods to ensure that the cleaning agent can effectively remove flux and has good compatibility with PCBs and components. For difficult-to-clean solder joints or local residues, ultrasonic cleaning or other special cleaning technologies can be considered.
  • Improve Quality Control and Inspection: Strengthen the quality control process to ensure the correct application of low-temperature solder paste and the stability of the soldering process. Use appropriate inspection methods and tools, such as X-ray inspection or microscopic examination, to identify and correct flux residue problems.
  • Enhance Supply Chain Management: Cooperate with suppliers to ensure that the purchased low-temperature solder paste and flux meet the requirements and have quality and reliability guarantees. Establish a sound supply chain management system to ensure the stable supply and quality consistency of raw materials.
  • Training and Technical Support: Train operators to make them understand the characteristics of low-temperature solder paste and flux and the correct usage methods. Cooperate with suppliers or professional technical support personnel to obtain technical support and suggestions to solve flux residue problems.